Silicone Aluminum Powder High Temperature Finish Paint
Silicone Aluminum Powder High Temperature Finish Paint
Silicone aluminum powder high temperature finish paint is prepared from silicone high-temperature resistant resin, aluminum powder, additives, solvents, etc. It is self-drying, does not need to be baked to dry, and has excellent high-temperature resistance. Mainly used to paint steel parts of high-temperature equipment, such as engine casing, chimney, exhaust pipe, oven, stove, etc.
Advantages of Silicone Aluminum Powder High Temperature Finish Paint
l Quick drying, excellent physical and mechanical properties
l Excellent heat resistance
l Excellent resistance to weather
l Good workability.
Specification of Silicone Aluminum Powder High Temperature Finish Paint
Type
Solvent
Solid Content
35%
Mixing Ratio
two components Part A : Part B=16:4 by weight
Dry Film Thickness
25μm per coat
Specific Gravity
1.0 kg/Liter
Coverage Rate (Theoretical)
0.09kg/m2/25μm 0.09L/m2/25μm
Drying Time
Temperature
10℃
20℃
30℃
Dry to touch
80mins
60mins
40mins
Dry Hard
8hrs
7hrs
6hrs
Package
20kgs for one kit, part A 16kgs, part B 4kgs
https://www.paint-in-china.com/uploads/image/20210129/20/high-temperature-finish.jpg